项目简介: The disclosure relates to a method for preparing titanium sponge, and in particular to a method for cyclically preparing titanium sponge and coproducing potassium cryolite using potassium fluotitanate as intermediate material. Titaniferous iron concentrate is the main mineral raw material for extracting titanium.

The existing titanium sponge preparation method takes the titaniferous iron concentrate as an initial material, obtains a rich-titanium material through a reducing smelting process, a chlorinated melting process, a pre-reduction hydrochloric acid leaching process, or a pre-reduction sulphuric acid leaching process. Titanium tetrachloride, which is formed by reacting the rich-titanium material with coke and chlorine gas at a high temperature of about 1000 °C, is used as an intermediate material. Then, the titanium sponge is prepared through a magnesium thermic reduction process (Kroll process) or a sodium thermic reduction process (Hunter process), wherein the reducing smelting process needs a high temperature of between 1700 and 1800 °C and obtains the rich-titanium material after using coke to perform reduction; the chlorinated melting process needs a high temperature of about 1000 °C and obtains the rich-titanium material after using coke and chlorine gas to perform reaction; the pre-reduction hydrochloric acid leaching process needs to be carried out at a high temperature of about 1200 °C, and uses hydrochloric acid to perform leaching after using coke to perform pre-reduction, and then heats and dehydrates the titanic acid formed to obtain the rich-titanium material; the pre-reduction sulphuric acid leaching process needs to be carried out at a high temperature of about 1200 °C, and uses sulphuric acid to perform leaching after using coke to perform pre-reduction, and then heats and dehydrates the titanic acid formed to obtain the rich-titanium material.

The titanium tetrachloride will generate corresponding coproduct chlorate while preparing titanium sponge through the magnesium thermic reduction process (Kroll process) or the sodium thermic reduction process (Hunter process). It is necessary to adopt a melting electrolytic method to separate and recycle the metal and chlorine gas.

项目核心创新点: - Cyclically preparing titanium sponge and coproducing potassium cryolite - Utilization of potassium fluotitanate as an intermediate material - Enhanced efficiency and reduced environmental impact through optimized processes

项目详细用途: - Production of high-quality titanium sponge - Synthesis of potassium cryolite as a byproduct - Potential applications in various industries, including aerospace, automotive, and chemical manufacturing

预期效益说明: - Improved economic efficiency due to the coproduction of potassium cryolite - Reduced energy consumption and environmental pollution - Enhanced titanium sponge production capacity and quality - Strengthened competitiveness in the global titanium industry

(此文字表达经过AI优化完善,查看原文请点击 原文)